Why may the boiler or incinerator refractory lining surface of the firebrick break away in layers?

21 Oct '18, 23:00

Oct. 21, 2018, 11 p.m.
KnowledgeBase's gravatar image



Answer:

Slagging occurs due to the fluctuation of temperatures in the furnace. To prevent it the furnace temperature fluctuations to be minimized.