The seating surface of a superheater handhole door on a boiler has been damaged due to leakage of superheated steam leaving a cut across the surface. Which repair method, would be appropriate?

06 May '20, 03:59

May 6, 2020, 3:59 a.m.
3Eng's gravatar image




Answer:

Build up the cut with weld and re-machine the seat.